Maka rino Te hiko hiko ENi-Cl Welding mea
KAUPAPA KAUPAPA:
KONO(wt%) | C | Mn | Si | Ni | Fe | Al | Cu | P | S |
GB/T RULES | 2.00 | 1.00 | 2.50 | ≥90 | 8.00 | - | - | - | 0.03 |
Nga Ture AWS | 2.00 | 2.50 | 4.00 | ≥85 | 8.00 | 1.00 | 2.50 | - | 0.03 |
UARA TAUIRA | 0.23 | 0.16 | 0.97 | 97.2 | 1.1 | 0.24 | 0.01 | 0.024 | 0.003 |
TE KAUPAPA MAHI:
WHAI | KAUPAPA KAUPAPA(MPa) | TE KAUPAPA KAUPAPA(MPa) | WARA WHAKAMAHI J/℃ | WHAKARANGA(%) | ||||
GB/T RULES | - | - | - | - | ||||
Nga Ture AWS | - | - | - | - | ||||
UARA TAUIRA | - | - | - | - |
NGĀ TAWHE WELDING E WHAKATAHIngia ana:
NGĀ WHAKATAKITANGA (mm) | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | ||||
HIKO(Amp) | H/W | 60-80 | 70-120 | 100-150 | 130-170 |
Ko te electrode he parakore nickel matua, kaha graphitized maka hiko rino;
A, no te fehokotaki'anga, e kore e taea te preheated te weldment;
Ko te kaitao he momo rino maatao te rino me te pai ake o nga mahi matawhānui penei i te aukati kapiti, te taonga miihini, te whakahaere me nga taonga miihini.
-
CJ50 keri keri-ake
-
Mei Jin Hua Sheng ethylene glycol pourewa waihanga
-
3000m te papa keri wai-rua-roto "Haiyang Shiyou 981"
KAUPAPA KAUPAPA:
KONO(wt%) | C | Mn | Si | Ni | Fe | Al | Cu | P | S |
GB/T RULES | 2.00 | 1.00 | 2.50 | ≥90 | 8.00 | - | - | - | 0.03 |
Nga Ture AWS | 2.00 | 2.50 | 4.00 | ≥85 | 8.00 | 1.00 | 2.50 | - | 0.03 |
UARA TAUIRA | 0.23 | 0.16 | 0.97 | 97.2 | 1.1 | 0.24 | 0.01 | 0.024 | 0.003 |
TE KAUPAPA MAHI:
WHAI | KAUPAPA KAUPAPA(MPa) | TE KAUPAPA KAUPAPA(MPa) | WARA WHAKAMAHI J/℃ | WHAKARANGA(%) | ||||
GB/T RULES | - | - | - | - | ||||
Nga Ture AWS | - | - | - | - | ||||
UARA TAUIRA | - | - | - | - |
NGĀ TAWHE WELDING E WHAKATAHIngia ana:
NGĀ WHAKATAKITANGA (mm) | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | ||||
HIKO(Amp) | H/W | 60-80 | 70-120 | 100-150 | 130-170 |
Tuhia to korero ki konei ka tukuna mai ki a matou